Formulating Stable DTF and Powderless GTF Aqueous Inks: Self-Dispersed Pigment Selection & Printhead Reliability Guide

Choose a self-dispersed pigment for DTF or powderless GTF by testing it in the ink that will actually pass through the intended Epson I3200 or S3200 aqueous printhead. Start with two grades of the same Colour Index at equal pigment loading. Add the intended humectants and polyurethane binder, then check how D90 and D97, viscosity and filter throughput change. A small D50 can coexist with a few agglomerates large enough to load a filter. An ink that jets cleanly can still peel from a garment after washing. Qualify those outcomes separately. The cyan pair below gives an ink maker a practical starting point. Both use PB15:3 at 15 wt% pigment, so the formulation trial can focus on differences between the two grades.

Where does the adhesive enter the transfer?

In conventional direct-to-film (DTF) printing, hot-melt powder is applied to the wet print, heated and then pressed onto fabric. For a colour trial, hold film, white backing, powder coverage and press conditions constant. In the glue-to-film (GTF) process described by Yilijet, the printer deposits adhesive through a dedicated channel. Include adhesive coverage, registration and the time between layers in that trial. The pigment supplies the colour. The adhesive layer has to hold it to the garment. Some powderless machines instead use inks with an integrated bonding function. Establish which fluid carries the binder before you screen a new dispersion. Mimaki DTF process · Yilijet GTF process · DCC integrated-ink example

What changes when humectants and polyurethane enter the ink?

Surface-grafted hydrophilic groups let a self-dispersed grade disperse in water without a separate polymeric dispersant. That changes the polymer budget. To find out whether it lowers viscosity, compare it with a polymer-dispersed control at equal pigment loading and binder solids. Ionised surface groups help particles repel one another in water. Adding a humectant changes the liquid surrounding the particles. Solvent shock can occur during mixing when a local excess of co-solvent exposes the pigment to a much higher concentration than the final recipe specifies. Water loss at an idle nozzle can also concentrate the remaining ingredients. In a published experiment, a surface-functionalised pigment remained dispersed over only part of the tested water, glycerol and 1,6-hexanediol mixtures. Annable, Lozman and Ewing, Figure 6

Prepare three matched samples using pigment in the water/humectant blend, polyurethane (PU) binder in that blend, and the complete ink. If only the complete ink forms specks, measure pH before and after mixing. A pH shift can change surface charge, and dissolved salts can screen electrostatic repulsion. A binder that carries the opposite charge may co-flocculate with the pigment. If specks appear before the binder addition, compare premixing the humectant with water against the original addition order. Vary glycerol, propylene glycol or 2-pyrrolidone individually and record pH, conductivity and any change in filter throughput.

Compare carboxylic and phosphate dispersions at equal pigment loading

Selected 15 wt% AIC concentrates. Each particle-size triplet is one sample’s D50 / D90 / D97 in nanometres.
Evaluation dimensionCarboxylicPhosphateSelection consequence
Candidate gradesCyan 6900 (PB15:3), Magenta Pink K6B (PV19), Black 0058 (PBk7)Cyan HC-7533 (PB15:3), Black 9003 (PBk7)Pair cyan with cyan or black with black to control for pigment identity.
Co-solvent and PU compatibilityChallenge the carboxylic grade with the intended PU dispersion and humectant blend.Repeat at the same pH, solvent fraction and binder solids. Include the actual production water.Rank each pair by changes after blending and storage. Neither surface chemistry establishes compatibility across PU grades.
Measured sample sizes (nm)6900: 141 / 197 / 228
K6B: 145 / 200 / 230
0058: 127 / 172 / 199
HC-7533: 157 / 208 / 239
9003: 126 / 170 / 196
The black medians differ by just 1 nm. Give filtration and restart results more weight when choosing between them.
Concentrate viscosity≤3 mPa·s for the three listed grades≤3 mPa·s for the two listed gradesMeasure the finished ink at the printer’s operating temperature after adding PU and humectants.

Use the AIC grade comparison by Colour Index to find carboxylic and phosphate grades based on the same pigment. For a conventional DTF trial, start with the DTF colour and white dispersion shortlist.

D97 describes the diameter below which 97% of the reported distribution falls. A larger agglomerate can still be present. For direct comparisons, match the sizing method, distribution basis and dilution. Original AIC particle-size reports · Grade-specific technical data sheets

Six AIC dispersion grades for an initial ink trial

The table describes aqueous concentrates as supplied. For a comparison of carboxylic (–COOH) and phosphoric acid (–PO₃H₂) surface groups, begin with the two PB15:3 cyan grades. Hold pigment loading, binder solids, pH and the humectant blend constant. Select candidates against the finished-ink trials below.

Nominal pigment content, concentrate viscosity from the TDS and D50 with its source
AIC gradePigment and surface groupsPigment contentViscosity (mPa·s)D50 (nm)Technical data
AIC-Cyan 6900PB15:3 · Carboxylic15 wt%≤3141 · sampleTDS (PDF)
AIC-Cyan HC-7533PB15:3 · Phosphate15 wt%≤3157 · sampleTDS (PDF)
AIC-Magenta Pink K6BPV19 · Carboxylic15 wt%*≤3145 · sampleTDS (PDF)
AIC-Yellow 2024PY155 · Carboxylic15 wt%≤3136 · sampleTDS (PDF)
AIC-Black 0058PBk7 · Carboxylic15 wt%≤3127 · sampleTDS (PDF)
AIC-WHITE S701
Development grade
TiO₂ · Carboxylic and phosphoric acid groups60% TiO₂9.5–12≈280 · TDS typicalTDS (PDF)

*K6B’s product page gives its nominal pigment content. The five colour and black rows link to individual sample reports. S701’s D50 is a typical TDS value. Contact AIC to confirm availability for white-ink evaluation.

Four tests before an Epson I3200 or S3200 production trial

Check the complete head designation first. Epson lists reference viscosity ranges of 2.2–4.5 mPa·s for the aqueous I3200(4)-A1, 3.2–4.4 for the S3200-A1 and 5.0–7.0 for the S3200-A3. Confirm the operating conditions with the printer integrator. Epson I3200 specifications · Epson S3200 specifications

  1. Coarse particle tail and filterability. Compare D90 and D97 after the binder and humectants have been added. Use the same particle-sizing method, distribution basis and sample preparation for the trial and reference inks. Pass equal masses through identical membranes at a fixed pressure and temperature. Time successive equal fractions and inspect the residue. Progressively slower flow can reveal developing filter loading even when D50 barely changes. Repeat after ageing.
  2. Accelerated ageing at 60 °C. Use separate sealed aliquots for days 0, 7 and 14 of a 60 °C challenge, alongside an ambient control. Return samples to the same measurement temperature. Track D50, D97, viscosity drift, pH and filter time. A project might target a D50 drift below 10% (100 × |D50 after ageing − initial D50| / initial D50) and pH 7.5–9.0. Set limits against a qualified reference. The Cyan 6900 concentrate TDS separately specifies seven days at 60 °C and a viscosity-change target of ≤10%. This accelerated comparison does not establish a shelf life. Cyan 6900 TDS
  3. White-ink settling and recovery. AIC-WHITE S701 is a development-grade concentrate containing 60% TiO₂. In the formulated white ink, track sediment height and the mixing needed to redisperse it. After a fixed rest, compare top and bottom samples and print white patches on the same dark backing. Check whether a binder or rheology adjustment that reduces settling still allows clean jetting. S701 evaluation data
  4. Dynamic surface tension, decap and first-drop recovery. Measure the finished ink and the reference with a maximum bubble-pressure tensiometer or another method qualified for the required surface ages. Record surface tension (mN/m) against surface age (time since a fresh interface formed) at a controlled temperature. Compare the inks at matched ages within the instrument’s validated range. Check drop breakup at the intended waveform and firing rate, then check dot spread and coalescence on the actual coated film. A concentrate’s static surface tension is a separate incoming-material measurement. AIC dynamic surface tension guide · Drop-on-demand surface tension study

    On an approved test stand, run a high-duty pattern at the intended firing frequency and duration. Record the active nozzle count and drop direction before and after the run. For a decap test, idle uncapped for 10, 20 and 30 minutes where permitted by the integrator. At each restart, divide the number of nozzles that fire a clean first drop before purging by the baseline active count. Report the percentage. Record temperature and humidity, missing or deflected first drops, and recovery after a fixed purge. Epson uses piezoelectric actuation. Inspect the nozzle face for dried ink and wetting defects when diagnosing dropout. In thermal inkjet, the term kogation refers to deposits on a firing resistor. Study of thermal inkjet deposits. Epson actuation principle

Qualify the transferred garment separately. Press matched colour patches and fine lines onto the target fabric, record coverage and edge lift, then repeat the assessment after a stated wash and drying programme. Record colour loss, staining, cracks and adhesive failure separately. ISO 6330 washing and drying procedures · ISO 105-C06 colour fastness to laundering

DTF and GTF formulation questions

Why does DTF ink clog Epson I3200 printheads after adding polyurethane resin?

A pH shift or a change in ionic strength after PU addition can destabilise the pigment. The binder can also introduce agglomerates of its own or raise viscosity enough to impair refill. Compare the binder alone, pigment alone and complete ink in the same vehicle. Filter residue, viscosity and first-drop behaviour help distinguish these causes.

What D50 and D97 particle size targets are safe for DTF pigment inks?

The five AIC colour and black samples in the platform comparison span 126–157 nm D50 and 196–239 nm D97. These sample measurements do not establish a universal nozzle limit. Qualify the finished ink by filtration, ageing and repeated nozzle-recovery checks on the intended head.

How to evaluate AIC pigment dispersions before scaling up?

Start with a 500 mL–1 L sample bottle, its lot-specific certificate of analysis and the corresponding particle-size distribution. Compare the grade with a production reference at equal pigment loading, then document filterability, idle recovery and post-wash transfer performance. Request a formulation sample.

Request a dispersion shortlist for your transfer ink

Tell us your printhead, required colours and transfer process. Request a 500 mL–1 L evaluation sample per bottle, the grade-specific TDS and SDS, and the COA and particle-size report for the evaluation lot where available. Browse technical and safety documents · View a representative COA

Your enquiry will be sent securely to AIC (Hangzhou Iris Chemical Technology Co., Ltd.). Privacy Policy